Use:
Brady-565 is designed for applications like identification labels or rating and serial plates that utilize barcodes, alphanumerics, graphic symbols and logos and require nameplate-like quality.
Substrate Type:
Matte Metallized Polyester
Adhesive Type:
Permanent pressure sensitive acrylic
Standard Material Colors:
Matte Metallized
Thickness (PSTC-33):
.0028 in. (.07 mm)
Adhesive Properties:
Adhesion to Steel (PSTC-1)
15 Minute Dwell (Avg.) -73oz/in. ( 80 N/100mm)
Ultimate Dwell (72 Hrs.) (Avg.) - 78 oz/in. (85 N/100mm)
Tack (ASTM D 2979) (Avg.) - 1444g. ( 14 N)
Abrasion Resistance (Method 5306 of U.S. Federal Test Method Std. No. 191A):
CS-10 wheels, 250 g wts.
The printed legend withstands up to 230 cycles.
Gloss (ASTM D523):
60° -101 Gardner Units
Minimum Application Temperature:
°0F (-18°C)
Service Temperature:
-40°F to 230°F (-40°C to 110°C)
Average Outdoor Durability:
3-5 years (Average expected outdoor life of product will depend on user definition of failure, climatic conditions, mounting techniques and material color.)
Chemical Resistance:
|
REAGENT
|
7 DAY IMMERSION
|
DIP TEST
|
RUB TEST
|
| 30% Sulfuric Acid |
NE
|
NE
|
NE
|
| 10% Sulfuric Acid |
F
|
NE
|
NE
|
| 30% Hydrochloric Acid |
NE
|
NE
|
NE
|
| 10% Hydrochloric Acid |
NE
|
NE
|
NE
|
| Glacial Acetic Acid |
F
|
F
|
F
|
| 5% Acetic Acid |
NE
|
NE
|
NE
|
| 50% Sodium Hydroxide |
F
|
NE
|
NE
|
| 10% Sodium Hydroxide |
F
|
NE
|
NE
|
| 10% Ammonia |
NE
|
NE
|
NE
|
| 5% Sodium Hypochlorite |
NE
|
NE
|
NE
|
| Methyl Ethyl Ketone |
F
|
F
|
F
|
| Acetone |
F
|
F
|
F
|
| Toluene |
F
|
F
|
F
|
| 1,1,1-Trichloroethane |
F
|
F
|
F
|
| Methanol |
NE
|
NE
|
NE
|
| Isopropyl Alcohol |
F
|
NE
|
NE
|
| Heptane |
NE
|
NE
|
NE
|
| Mineral Spirits |
NE
|
NE
|
NE
|
| Turpentine |
F
|
NE
|
NE
|
| Kerosene |
NE
|
NE
|
NE
|
| Diesel Fuel |
NE
|
NE
|
NE
|
| Gasoline |
F
|
NE
|
F
|
| ASTM #3 Oil |
NE
|
NE
|
NE
|
| SAE 20 Oil |
NE
|
NE
|
NE
|
| 10% Sodium Chloride |
NE
|
NE
|
NE
|
| Alconox® |
NE
|
NE
|
NE
|
| Water |
NE
|
NE
|
NE
|
NE = No Effect
F = Failed (affected Sample)
7 Day Immersion: Immersed in reagent for 7 days.
Dip Test: Five 10 minute dips in reagent with 30 minute recovery.
Rub Test: Rubbed sample for 1 minute with swab soaked in reagent.
Product testing, customer feedback, and history of similar products, support a customer performance expectation of at least two years from the date of receipt for this product as long as this product is stored in its original packaging in an environment below 80°F (27°C) and 60% RH . We are confident that our product will perform well beyond this time frame. However, it remains the responsibility of the user to assess the risk of using such product. We encourage customers to develop functional testing protocols that will qualify a product's fitness for use in their actual applications.